Question:Two previously undeformed cylindrical specimens of an alloy
are to be strain hardened by reducing their...
Question
Two previously undeformed cylindrical specimens of an alloy
are to be strain hardened by reducing their...
Two previously undeformed cylindrical specimens of an alloy
are to be strain hardened by reducing their cross-sectional areas
(while maintaining their circular cross sections). For one
specimen, the initial and deformed radii are 15 and 11 mm,
respectively. The second specimen, with an initial radius of 11 mm,
must have the same deformed hardness as the first specimen; compute
the second specimen’s radius (in mm) after deformation.