Ceramic To produce a strong ceramic piece, silicon carbide particles are compacted and baked at high...

Ceramic
To produce a strong ceramic piece, silicon carbide particles are compacted and baked at high temperature. The specific gravity of SiC is 3.2g / cm3. The ceramic piece is weighed respectively when dry (200 g), after soaking in water (223 g) and while suspended in water (211 g). Calculate the apparent porosity, actual porosity, and volume fraction of pores that are closed.